The dielectric and piezoelectric properties of high Curie temperature 0.6Pb(Yb1/2Nb1/2)O3-0.4PbTiO3 (PYNT40) single crystals as a function of temperature are reported. The Curie temperature of PYNT40 single crystals was about 270°C and the rhombohedral to tetragonal phase transition temperature was ∼168°C. The piezoelectric and electromechanical coupling coefficients at room temperature were d33∼1200pC/N, k33∼88%, d31∼ -500 pC/N, k31∼ -76% and d15∼1700pC/N, k15∼88%, respectively. The coupling coefficients remained nearly constant until ∼160°C, indicating improved temperature stability compared to Pb(Zn1/3Nb2/3)O3-PbTiO3 and Pb(Mg1/3Nb2/3)O3-PbTiO3 single crystals.

Original languageEnglish (US)
Pages455-458
Number of pages4
StatePublished - Dec 1 2002
EventProceedings of the 13th IEEE International Symposium on Applications of Ferroelectronics - Nara, Japan
Duration: May 28 2002Jun 1 2002

Other

OtherProceedings of the 13th IEEE International Symposium on Applications of Ferroelectronics
CountryJapan
CityNara
Period5/28/026/1/02

    Fingerprint

All Science Journal Classification (ASJC) codes

  • Electronic, Optical and Magnetic Materials
  • Electrical and Electronic Engineering

Cite this

Zhang, S., Lebrun, L., Rhee, S., Randall, C. A., & Shrout, T. R. (2002). Dielectric and piezoelectric properties as a function of temperature for Pb(Yb1/2Nb1/2)O3-PbTiO3 single crystals. 455-458. Paper presented at Proceedings of the 13th IEEE International Symposium on Applications of Ferroelectronics, Nara, Japan.