Magnesium doped potassium lithium niobate single crystal was grown by using pulling method. The dielectric properties of c and a slice at 10-700 K were studied. The dependence of dielectric constant on temperature in 5×102-5×108 Hz was obtained. Results showed ferroelectric-paraelectric phase transition happened at 623 K and a ferroelectric phase transition at 80 K. The dielectric relaxation is 250 Hz.

Original languageEnglish (US)
Pages (from-to)393-394
Number of pages2
JournalGongneng Cailiao/Journal of Functional Materials
Volume32
Issue number4
StatePublished - Aug 1 2001

Fingerprint

lithium niobates
Dielectric properties
Magnesium
Ferroelectric materials
Potassium
magnesium
dielectric properties
potassium
Lithium
Phase transitions
Single crystals
Dielectric relaxation
single crystals
pulling
Permittivity
permittivity
Temperature
temperature
lithium niobate

All Science Journal Classification (ASJC) codes

  • Electronic, Optical and Magnetic Materials
  • Condensed Matter Physics
  • Electrical and Electronic Engineering
  • Materials Chemistry

Cite this

Cheng, Z. X., Zhang, S., Chen, H. C., Zhang, P. L., & Zhong, W. L. (2001). Growth and dielectric property of magnesium doped potassium lithium niobate single crystal. Gongneng Cailiao/Journal of Functional Materials, 32(4), 393-394.
Cheng, Zhen Xiang ; Zhang, Shujun ; Chen, Huan Chu ; Zhang, Pei Lin ; Zhong, Wei Lie. / Growth and dielectric property of magnesium doped potassium lithium niobate single crystal. In: Gongneng Cailiao/Journal of Functional Materials. 2001 ; Vol. 32, No. 4. pp. 393-394.
@article{2084f7c2629b4b83abe7edfc90f1d0c9,
title = "Growth and dielectric property of magnesium doped potassium lithium niobate single crystal",
abstract = "Magnesium doped potassium lithium niobate single crystal was grown by using pulling method. The dielectric properties of c and a slice at 10-700 K were studied. The dependence of dielectric constant on temperature in 5×102-5×108 Hz was obtained. Results showed ferroelectric-paraelectric phase transition happened at 623 K and a ferroelectric phase transition at 80 K. The dielectric relaxation is 250 Hz.",
author = "Cheng, {Zhen Xiang} and Shujun Zhang and Chen, {Huan Chu} and Zhang, {Pei Lin} and Zhong, {Wei Lie}",
year = "2001",
month = "8",
day = "1",
language = "English (US)",
volume = "32",
pages = "393--394",
journal = "Gongneng Cailiao/Journal of Functional Materials",
issn = "1001-9731",
publisher = "Journal of Functional Materials",
number = "4",

}

Cheng, ZX, Zhang, S, Chen, HC, Zhang, PL & Zhong, WL 2001, 'Growth and dielectric property of magnesium doped potassium lithium niobate single crystal', Gongneng Cailiao/Journal of Functional Materials, vol. 32, no. 4, pp. 393-394.

Growth and dielectric property of magnesium doped potassium lithium niobate single crystal. / Cheng, Zhen Xiang; Zhang, Shujun; Chen, Huan Chu; Zhang, Pei Lin; Zhong, Wei Lie.

In: Gongneng Cailiao/Journal of Functional Materials, Vol. 32, No. 4, 01.08.2001, p. 393-394.

Research output: Contribution to journalArticle

TY - JOUR

T1 - Growth and dielectric property of magnesium doped potassium lithium niobate single crystal

AU - Cheng, Zhen Xiang

AU - Zhang, Shujun

AU - Chen, Huan Chu

AU - Zhang, Pei Lin

AU - Zhong, Wei Lie

PY - 2001/8/1

Y1 - 2001/8/1

N2 - Magnesium doped potassium lithium niobate single crystal was grown by using pulling method. The dielectric properties of c and a slice at 10-700 K were studied. The dependence of dielectric constant on temperature in 5×102-5×108 Hz was obtained. Results showed ferroelectric-paraelectric phase transition happened at 623 K and a ferroelectric phase transition at 80 K. The dielectric relaxation is 250 Hz.

AB - Magnesium doped potassium lithium niobate single crystal was grown by using pulling method. The dielectric properties of c and a slice at 10-700 K were studied. The dependence of dielectric constant on temperature in 5×102-5×108 Hz was obtained. Results showed ferroelectric-paraelectric phase transition happened at 623 K and a ferroelectric phase transition at 80 K. The dielectric relaxation is 250 Hz.

UR - http://www.scopus.com/inward/record.url?scp=0035435714&partnerID=8YFLogxK

UR - http://www.scopus.com/inward/citedby.url?scp=0035435714&partnerID=8YFLogxK

M3 - Article

AN - SCOPUS:0035435714

VL - 32

SP - 393

EP - 394

JO - Gongneng Cailiao/Journal of Functional Materials

JF - Gongneng Cailiao/Journal of Functional Materials

SN - 1001-9731

IS - 4

ER -