Abstract

A new method for the construction of high-temperature superconducting magnetic shielding structures has been demonstrated. With this process, a ceramic laminate of high-temperature superconducting powder and silver metal sheets is formed and then shaped into a cylindrical magnetic shield by deep drawing before being sintered. Two types of superconducting powders were used in this experiment, YBa2Cu3O7 and Bi1.8Pb0.4Sr2Ca2Cu3O x, which exhibited shielding factors of 1100 and 330, respectively.

Original languageEnglish (US)
Pages (from-to)50-54
Number of pages5
JournalIEEE Transactions on Applied Superconductivity
Volume6
Issue number1
DOIs
StatePublished - Dec 1 1996

Fingerprint

deep drawing
Deep drawing
Powders
Magnetic shielding
magnetic shielding
metal sheets
Sheet metal
Silver
Shielding
laminates
Laminates
shielding
silver
ceramics
Temperature
Experiments
barium copper yttrium oxide

All Science Journal Classification (ASJC) codes

  • Electrical and Electronic Engineering
  • Physics and Astronomy (miscellaneous)

Cite this

Johnson, Deonna F. ; Opie, David B. ; Schone, Harlan E. ; Lanagan, Michael T. ; Stevens, Jonathan C. / High-temperature superconducting magnetic shields formed by deep drawing. In: IEEE Transactions on Applied Superconductivity. 1996 ; Vol. 6, No. 1. pp. 50-54.
@article{5c1145d43b414df988760637c0690a5f,
title = "High-temperature superconducting magnetic shields formed by deep drawing",
abstract = "A new method for the construction of high-temperature superconducting magnetic shielding structures has been demonstrated. With this process, a ceramic laminate of high-temperature superconducting powder and silver metal sheets is formed and then shaped into a cylindrical magnetic shield by deep drawing before being sintered. Two types of superconducting powders were used in this experiment, YBa2Cu3O7 and Bi1.8Pb0.4Sr2Ca2Cu3O x, which exhibited shielding factors of 1100 and 330, respectively.",
author = "Johnson, {Deonna F.} and Opie, {David B.} and Schone, {Harlan E.} and Lanagan, {Michael T.} and Stevens, {Jonathan C.}",
year = "1996",
month = "12",
day = "1",
doi = "10.1109/77.488281",
language = "English (US)",
volume = "6",
pages = "50--54",
journal = "IEEE Transactions on Applied Superconductivity",
issn = "1051-8223",
publisher = "Institute of Electrical and Electronics Engineers Inc.",
number = "1",

}

High-temperature superconducting magnetic shields formed by deep drawing. / Johnson, Deonna F.; Opie, David B.; Schone, Harlan E.; Lanagan, Michael T.; Stevens, Jonathan C.

In: IEEE Transactions on Applied Superconductivity, Vol. 6, No. 1, 01.12.1996, p. 50-54.

Research output: Contribution to journalArticle

TY - JOUR

T1 - High-temperature superconducting magnetic shields formed by deep drawing

AU - Johnson, Deonna F.

AU - Opie, David B.

AU - Schone, Harlan E.

AU - Lanagan, Michael T.

AU - Stevens, Jonathan C.

PY - 1996/12/1

Y1 - 1996/12/1

N2 - A new method for the construction of high-temperature superconducting magnetic shielding structures has been demonstrated. With this process, a ceramic laminate of high-temperature superconducting powder and silver metal sheets is formed and then shaped into a cylindrical magnetic shield by deep drawing before being sintered. Two types of superconducting powders were used in this experiment, YBa2Cu3O7 and Bi1.8Pb0.4Sr2Ca2Cu3O x, which exhibited shielding factors of 1100 and 330, respectively.

AB - A new method for the construction of high-temperature superconducting magnetic shielding structures has been demonstrated. With this process, a ceramic laminate of high-temperature superconducting powder and silver metal sheets is formed and then shaped into a cylindrical magnetic shield by deep drawing before being sintered. Two types of superconducting powders were used in this experiment, YBa2Cu3O7 and Bi1.8Pb0.4Sr2Ca2Cu3O x, which exhibited shielding factors of 1100 and 330, respectively.

UR - http://www.scopus.com/inward/record.url?scp=0030105033&partnerID=8YFLogxK

UR - http://www.scopus.com/inward/citedby.url?scp=0030105033&partnerID=8YFLogxK

U2 - 10.1109/77.488281

DO - 10.1109/77.488281

M3 - Article

AN - SCOPUS:0030105033

VL - 6

SP - 50

EP - 54

JO - IEEE Transactions on Applied Superconductivity

JF - IEEE Transactions on Applied Superconductivity

SN - 1051-8223

IS - 1

ER -