Parametric study of temperature-modulated differential scanning calorimetry for high-temperature oxide glasses with varying fragility

Tobias K. Bechgaard, Ozgur Gulbiten, John C. Mauro, Morten M. Smedskjaer

Research output: Contribution to journalArticlepeer-review

4 Scopus citations

Fingerprint Dive into the research topics of 'Parametric study of temperature-modulated differential scanning calorimetry for high-temperature oxide glasses with varying fragility'. Together they form a unique fingerprint.