Abstract

YBa2Cu3Ox powders were sintered in sealed Ag and Ag/10% Pd wraps and melted on Ag/10% Pd foils. The melting was performed at 980°C under an O2 pressure of 103 Pa. Although YBa2Cu3Ox was successfully melt-processed, some interdiffusion occurred between it and the Ag Pd alloy. The superconducting transition temperature was 86-88 K for YBa2Cu3Ox processed with Ag Pd alloy and 89 K for YBa2Cu3Ox processed with pure Ag.

Original languageEnglish (US)
Pages (from-to)291-294
Number of pages4
JournalMaterials Letters
Volume12
Issue number4
DOIs
StatePublished - Jan 1 1991

Fingerprint

Palladium alloys
palladium alloys
Silver alloys
silver alloys
wrap
Powders
Metal foil
Superconducting transition temperature
foils
Melting
transition temperature
melting

All Science Journal Classification (ASJC) codes

  • Materials Science(all)
  • Condensed Matter Physics
  • Mechanics of Materials
  • Mechanical Engineering

Cite this

Risch, G. A. ; Lanagan, Michael T. ; Wu, W. ; Goretta, K. C. ; Moon, B. M. / YBa2Cu3Ox processed with a silver/palladium alloy. In: Materials Letters. 1991 ; Vol. 12, No. 4. pp. 291-294.
@article{4a5ed11596ad4b198ec39424c660ec39,
title = "YBa2Cu3Ox processed with a silver/palladium alloy",
abstract = "YBa2Cu3Ox powders were sintered in sealed Ag and Ag/10{\%} Pd wraps and melted on Ag/10{\%} Pd foils. The melting was performed at 980°C under an O2 pressure of 103 Pa. Although YBa2Cu3Ox was successfully melt-processed, some interdiffusion occurred between it and the Ag Pd alloy. The superconducting transition temperature was 86-88 K for YBa2Cu3Ox processed with Ag Pd alloy and 89 K for YBa2Cu3Ox processed with pure Ag.",
author = "Risch, {G. A.} and Lanagan, {Michael T.} and W. Wu and Goretta, {K. C.} and Moon, {B. M.}",
year = "1991",
month = "1",
day = "1",
doi = "10.1016/0167-577X(91)90016-Y",
language = "English (US)",
volume = "12",
pages = "291--294",
journal = "Materials Letters",
issn = "0167-577X",
publisher = "Elsevier",
number = "4",

}

Risch, GA, Lanagan, MT, Wu, W, Goretta, KC & Moon, BM 1991, 'YBa2Cu3Ox processed with a silver/palladium alloy', Materials Letters, vol. 12, no. 4, pp. 291-294. https://doi.org/10.1016/0167-577X(91)90016-Y

YBa2Cu3Ox processed with a silver/palladium alloy. / Risch, G. A.; Lanagan, Michael T.; Wu, W.; Goretta, K. C.; Moon, B. M.

In: Materials Letters, Vol. 12, No. 4, 01.01.1991, p. 291-294.

Research output: Contribution to journalArticle

TY - JOUR

T1 - YBa2Cu3Ox processed with a silver/palladium alloy

AU - Risch, G. A.

AU - Lanagan, Michael T.

AU - Wu, W.

AU - Goretta, K. C.

AU - Moon, B. M.

PY - 1991/1/1

Y1 - 1991/1/1

N2 - YBa2Cu3Ox powders were sintered in sealed Ag and Ag/10% Pd wraps and melted on Ag/10% Pd foils. The melting was performed at 980°C under an O2 pressure of 103 Pa. Although YBa2Cu3Ox was successfully melt-processed, some interdiffusion occurred between it and the Ag Pd alloy. The superconducting transition temperature was 86-88 K for YBa2Cu3Ox processed with Ag Pd alloy and 89 K for YBa2Cu3Ox processed with pure Ag.

AB - YBa2Cu3Ox powders were sintered in sealed Ag and Ag/10% Pd wraps and melted on Ag/10% Pd foils. The melting was performed at 980°C under an O2 pressure of 103 Pa. Although YBa2Cu3Ox was successfully melt-processed, some interdiffusion occurred between it and the Ag Pd alloy. The superconducting transition temperature was 86-88 K for YBa2Cu3Ox processed with Ag Pd alloy and 89 K for YBa2Cu3Ox processed with pure Ag.

UR - http://www.scopus.com/inward/record.url?scp=0026255770&partnerID=8YFLogxK

UR - http://www.scopus.com/inward/citedby.url?scp=0026255770&partnerID=8YFLogxK

U2 - 10.1016/0167-577X(91)90016-Y

DO - 10.1016/0167-577X(91)90016-Y

M3 - Article

VL - 12

SP - 291

EP - 294

JO - Materials Letters

JF - Materials Letters

SN - 0167-577X

IS - 4

ER -